4.0mm 316 Stainless Steel Cooking Grill Grate Bright Annealed Annealed 1Kg Spool
316 stainless steel grill grate
,4.0mm cooking grill grate
,bright annealed grill grate
Produced to JIS G4304, the wire pairs a Bright Annealed surface with a tensile range of 580-780 MPa, and every coil is traceable to its heat number. The wire is compatible with resistance welding, brazing and laser cutting, with no cracking at the fusion zone. The 316 grade offers chloride and marine grade corrosion resistance from the molybdenum addition, which is the reason it is chosen for parts exposed to moisture, cleaning agents or repeated wash down.
This Stainless Steel Cooking Grill Grate is drawn from 316 stainless steel at 4.0 and supplied in Annealed temper for buyers who need predictable forming behaviour. Coils are level wound with controlled cast and helix, so pay off tension stays even on automatic feeders.
Key Features- Stable Magnetic Response: The 316 grade is non-magnetic in the annealed condition, which matters for sensor, relay and magnetic clamping applications.
- Consistent Diameter Tolerance: Diameter is held to +/-0.03 mm across the whole coil and checked by laser micrometer every 50 m, so coiling and heading tools stay in setup without adjustment runs.
- Clean Degreased Coils: Coils are ultrasonically degreased and dried before packing, so plating or passivation lines need no extra pre cleaning step.
- Straightness and Coil Build: Level wound or spooled packing keeps the wire tangle free, so automatic feeders run without stoppage caused by coil collapse.
- Traceable Batch Records: Every lot carries heat number, drawing date, tensile record and surface inspection result, issued as an EN 10204 3.1 certificate on request.
- Verified Metallurgy: 316 chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
| Parameter | Specification |
|---|---|
| Steel Grade | 316 |
| Wire Diameter | 4.0 mm |
| Diameter Tolerance | ±0.03 mm |
| Surface Finish | Bright Annealed |
| Temper | Annealed |
| Tensile Strength | 580-780 MPa |
| Chemical Composition | 16.0-18.0% Cr, 10.0-14.0% Ni, 2.0-3.0% Mo |
| Standard | JIS G4304 |
| Coil Weight | 1 kg spool |
| Packing | VCI paper, strapping, wooden crate |
| Application | commercial restaurant grills |
| Delivery Time | 15-25 days after deposit |
Designers working on commercial restaurant grills value the strength and ductility balance of 316 in Annealed temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design. Because commercial restaurant grills often runs on high speed automatic equipment, wire that coils unevenly stops the line. The level winding and controlled cast of this Stainless Steel Cooking Grill Grate keep pay off tension constant, which is the practical reason repeat orders follow the first trial.
- Camping and picnic grills
- Commercial restaurant grills
- Charcoal and gas barbecue grills
- Smoker and pellet grill retrofit
- Outdoor kitchen cooking surfaces
Packing follows 1 kg spool as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving. Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally 1 kg spool, and neutral packing with your own label is available for distributors.
Product Q&AQ: What tensile range does Annealed temper give?
A: For 316 at 4.0 in Annealed temper the typical tensile range is 580-780 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.
Q: Can the grade be substituted to reduce cost?
A: In dry indoor work 201 often replaces 304 at lower cost, and 430 suits magnetic or high temperature domestic parts. For chloride, marine or food contact service we keep 316 or 316L to protect the end user.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.