4.0mm 304 Stainless Steel Spring Wire Soap Coated High Fatigue Life EN 10270-3
4.0mm 304 Spring Steel Wire
,Soap Coated SS Spring Wire
,Half Hard Wire Coil
Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section. Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record. The Soap Coated finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming.
Coils are level wound with controlled cast and helix, so pay off tension stays even on automatic feeders. Surface condition is monitored online, and finished coils are degreased before packing so plating lines receive clean material.
Key Features- Clean Degreased Coils: Coils are ultrasonically degreased and dried before packing, so plating or passivation lines need no extra pre cleaning step.
- Verified Metallurgy: 304 chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
- Fatigue Oriented Drawing: Multi pass drawing with intermediate annealing refines grain structure and limits inclusion stringers, extending fatigue life in cyclic spring and bending duty.
- {surf} Surface: A Soap Coated finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
- Stable Magnetic Response: The 304 grade is essentially non-magnetic in the annealed condition, which matters for sensor, relay and magnetic clamping applications.
- Custom Cut and Spool Options: Wire can be supplied on 1 kg spool, or cut to fixed lengths, matching your feeding equipment and stock policy.
| Parameter | Specification |
|---|---|
| Steel Grade | 304 |
| Wire Diameter | 4.0 mm |
| Diameter Tolerance | ±0.03 mm |
| Surface Finish | Soap Coated |
| Temper | Half Hard |
| Tensile Strength | 1,300-1,600 MPa |
| Chemical Composition | 18.0-20.0% Cr, 8.0-10.5% Ni |
| Standard | EN 10270-3 |
| Coil Weight | 1 kg spool |
| Packing | VCI paper, strapping, wooden crate |
| Application | door lock springs |
| Delivery Time | 15-25 days after deposit |
Designers working on door lock springs value the strength and ductility balance of 304 in Half Hard temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design. This Stainless Steel Spring Wire is specified where a supplier must guarantee the same mechanical result batch after batch, not just from a single sample. Buyers in door lock springs use it because drawing schedule, surface condition and temper are held inside a narrow window, keeping forming tools and assembly fixtures stable across long production runs.
- Industrial compression and torsion springs
- Washing machine idler springs
- Door lock springs
- Small appliance latch springs
- Medical and surgical instrument springs
Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally 1 kg spool, and neutral packing with your own label is available for distributors. Packing follows 1 kg spool as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving.
Product Q&AQ: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.
Q: Can the grade be substituted to reduce cost?
A: In dry indoor work 201 often replaces 304 at lower cost, and 430 suits magnetic or high temperature domestic parts. For chloride, marine or food contact service we keep 316 or 316L to protect the end user.
Q: Is the surface suitable for electroplating or PVD?
A: Yes. Bright finishes are degreased with surface roughness below 0.8 micrometre, so nickel, chrome or PVD layers build evenly. Soap coated wire needs a light alkaline clean before plating.