3.5mm 304 Stainless Steel Spring Wire Consistent Springback 100Kg Drum
3.5mm 304 Stainless Spring Wire
,Soap Coated SS Spring Wire
,Half Hard Wire Coil
Diameter control of +/-0.02 mm lets high speed coiling and heading equipment run without repeated tool adjustment between coils. Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section. The 304 grade offers broad atmospheric and food contact corrosion resistance, which is the reason it is chosen for parts exposed to moisture, cleaning agents or repeated wash down.
This Stainless Steel Spring Wire is drawn from 304 stainless steel at 3.5 and supplied in Half Hard temper for buyers who need predictable forming behaviour. Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders.
Key Features- Straightness and Coil Build: Level wound or spooled packing keeps the wire tangle free, so automatic feeders run without stoppage caused by coil collapse.
- Corrosion Performance: The 304 grade offers broad atmospheric and food contact corrosion resistance, verified by neutral salt spray testing of finished samples before dispatch.
- Dimensional Stability After Forming: Low residual stress from controlled drawing keeps formed parts inside print tolerance after springback and stress relief.
- {surf} Surface: A Soap Coated finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
- Custom Cut and Spool Options: Wire can be supplied on 100 kg drum, or cut to fixed lengths, matching your feeding equipment and stock policy.
- Smooth Surface for Plating: Surface roughness is held below 0.8 micrometre on bright finishes, so nickel, chrome or PVD layers build evenly.
| Parameter | Specification |
|---|---|
| Steel Grade | 304 |
| Wire Diameter | 3.5 mm |
| Diameter Tolerance | ±0.02 mm |
| Surface Finish | Soap Coated |
| Temper | Half Hard |
| Tensile Strength | 1,300-1,600 MPa |
| Chemical Composition | 18.0-20.0% Cr, 8.0-10.5% Ni |
| Standard | EN 10270-3 |
| Coil Weight | 100 kg drum |
| Packing | VCI paper, strapping, wooden crate |
| Application | sprayer and lotion pump springs |
| Delivery Time | 15-25 days after deposit |
Designers working on sprayer and lotion pump springs value the strength and ductility balance of 304 in Half Hard temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design. In sprayer and lotion pump springs the usual failure mode is fatigue or stress relaxation rather than simple overload. That is why this Stainless Steel Spring Wire is drawn from 304 with a refined grain structure and finished Soap Coated, so cyclic loading and warm service conditions do not shorten part life.
- Small appliance latch springs
- Automotive return springs
- Battery contact springs
- Door lock springs
- Washing machine idler springs
Standard export packing is 100 kg drum per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low. Packing follows 100 kg drum as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving.
Product Q&AQ: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.
Q: What is the minimum order quantity and lead time?
A: A trial order from 500 kg per size is accepted so you can validate forming behaviour. Repeat production quantities ship in 15 to 25 days after deposit, and stock sizes move within a week.
Q: What tensile range does Half Hard temper give?
A: For 304 at 3.5 in Half Hard temper the typical tensile range is 1,300-1,600 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.