8.0mm 304 Stainless Steel Cooking Grill Grate Bright Annealed ASTM A240
8.0mm 304 BBQ Cooking Grate
,Bright Annealed Cooking Grill Grate
,Bright Annealed Stainless Steel Cooking Grill
Produced to ASTM A240, the wire pairs a Bright Annealed surface with a tensile range of 600-800 MPa, and every coil is traceable to its heat number. Surface condition is monitored online, and finished coils are degreased before packing so plating lines receive clean material. Full traceability from melt to coil is maintained, including heat number, drawing date and final inspection signature.
Typical service covers springs, wire forms and fasteners where both strength and corrosion resistance are required. The wire is compatible with resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
Key Features- Welding and Fabrication Friendly: Balanced chemistry keeps the wire stable during resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
- Corrosion Performance: The 304 grade offers broad atmospheric and food contact corrosion resistance, verified by neutral salt spray testing of finished samples before dispatch.
- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 304 grade is routinely supplied for food contact and drinking water adjacent parts.
- Fatigue Oriented Drawing: Multi pass drawing with intermediate annealing refines grain structure and limits inclusion stringers, extending fatigue life in cyclic spring and bending duty.
- Controlled {temper} Temper: The wire is drawn to Annealed temper with a typical tensile range of 600-800 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
- Clean Degreased Coils: Coils are ultrasonically degreased and dried before packing, so plating or passivation lines need no extra pre cleaning step.
| Parameter | Specification |
|---|---|
| Steel Grade | 304 |
| Wire Diameter | 8.0 mm |
| Diameter Tolerance | ±0.03 mm |
| Surface Finish | Bright Annealed |
| Temper | Annealed |
| Tensile Strength | 600-800 MPa |
| Chemical Composition | 18.0-20.0% Cr, 8.0-10.5% Ni |
| Standard | ASTM A240 |
| Coil Weight | Z2 coil on cardboard core |
| Packing | VCI paper, strapping, wooden crate |
| Application | fire pit cooking grates |
| Delivery Time | 15-25 days after deposit |
Designers working on fire pit cooking grates value the strength and ductility balance of 304 in Annealed temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design. Export programmes for fire pit cooking grates demand consistent documentation and stable lead time. Production of this Stainless Steel Cooking Grill Grate is scheduled against a fixed rolling plan, with ASTM A240 testing and dimensional reports issued before the container is sealed.
- Outdoor kitchen cooking surfaces
- Fire pit cooking grates
- Charcoal and gas barbecue grills
- Smoker and pellet grill retrofit
- Camping and picnic grills
Packing follows Z2 coil on cardboard core as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving. Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally Z2 coil on cardboard core, and neutral packing with your own label is available for distributors.
Product Q&AQ: How do you prevent coil collapse during unwinding?
A: Coils are level wound with controlled cast and helix, then restrained with strapping and VCI film. For high speed feeders we recommend spooled packing, which keeps pay off tension constant.
Q: What tensile range does Annealed temper give?
A: For 304 at 8.0 in Annealed temper the typical tensile range is 600-800 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.
Q: Can the grade be substituted to reduce cost?
A: In dry indoor work 201 often replaces 304 at lower cost, and 430 suits magnetic or high temperature domestic parts. For chloride, marine or food contact service we keep 316 or 316L to protect the end user.