3.0mm 316 Stainless Steel Spring Wire Electrolysis Bright Bright Surface
3.0mm 316 Stainless Spring Wire
,Electrolysis Bright SS Spring Wire
,Half Hard Wire Coil
Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section. Diameter control of +/-0.02 mm lets high speed coiling and heading equipment run without repeated tool adjustment between coils. The Electrolysis Bright finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming.
Produced to EN 10270-3, the wire pairs a Electrolysis Bright surface with a tensile range of 1,250-1,550 MPa, and every coil is traceable to its heat number. Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders.
Key Features- Dimensional Stability After Forming: Low residual stress from controlled drawing keeps formed parts inside print tolerance after springback and stress relief.
- Welding and Fabrication Friendly: Balanced chemistry keeps the wire stable during resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
- Fatigue Oriented Drawing: Multi pass drawing with intermediate annealing refines grain structure and limits inclusion stringers, extending fatigue life in cyclic spring and bending duty.
- Custom Cut and Spool Options: Wire can be supplied on 10 kg coil, or cut to fixed lengths, matching your feeding equipment and stock policy.
- Controlled {temper} Temper: The wire is drawn to Half Hard temper with a typical tensile range of 1,250-1,550 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
- High Cycle Bending Endurance: Refined surface and clean microstructure reduce crack initiation sites, with sample lots tested beyond one million bending cycles.
| Parameter | Specification |
|---|---|
| Steel Grade | 316 |
| Wire Diameter | 3.0 mm |
| Diameter Tolerance | ±0.02 mm |
| Surface Finish | Electrolysis Bright |
| Temper | Half Hard |
| Tensile Strength | 1,250-1,550 MPa |
| Chemical Composition | 16.0-18.0% Cr, 10.0-14.0% Ni, 2.0-3.0% Mo |
| Standard | EN 10270-3 |
| Coil Weight | 10 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | door lock springs |
| Delivery Time | 15-25 days after deposit |
This Stainless Steel Spring Wire is specified where a supplier must guarantee the same mechanical result batch after batch, not just from a single sample. Buyers in door lock springs use it because drawing schedule, surface condition and temper are held inside a narrow window, keeping forming tools and assembly fixtures stable across long production runs. Purchasing teams sourcing for door lock springs compare three things: dimensional consistency, surface cleanliness and documentation. This coil answers all three, with +/-0.02 mm diameter control, a degreased Electrolysis Bright surface and a heat number linked mill certificate for every lot.
- Small appliance latch springs
- Watch band and jewellery springs
- Battery contact springs
- Medical and surgical instrument springs
- Telecom connector springs
Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally 10 kg coil, and neutral packing with your own label is available for distributors. Standard export packing is 10 kg coil per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low.
Product Q&AQ: What tensile range does Half Hard temper give?
A: For 316 at 3.0 in Half Hard temper the typical tensile range is 1,250-1,550 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.
Q: Is customised chemistry or coating available?
A: Yes. We can adjust carbon and nitrogen within grade limits, apply soap, wax or polymer lubricant coatings, and print your brand on the spool flange for distributor programmes.
Q: How do you prevent coil collapse during unwinding?
A: Coils are level wound with controlled cast and helix, then restrained with strapping and VCI film. For high speed feeders we recommend spooled packing, which keeps pay off tension constant.