0.3mm 430 Fine Stainless Steel Wire Half Hard Long Cycle Endurance 10Kg Coil
0.3mm 430 Fine Gauge SS Wire
,Bright Annealed Ultra Fine SS Wire
,Half Hard Wire Coil
Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section. Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders. Full traceability from melt to coil is maintained, including heat number, drawing date and final inspection signature.
The wire is compatible with resistance welding, brazing and laser cutting, with no cracking at the fusion zone. This Fine Stainless Steel Wire is drawn from 430 stainless steel at 0.3 and supplied in Half Hard temper for buyers who need predictable forming behaviour.
Key Features- Corrosion Performance: The 430 grade offers good oxidation and heat scaling resistance in domestic and appliance environments, verified by neutral salt spray testing of finished samples before dispatch.
- Stable Magnetic Response: The 430 grade is ferromagnetic, which suits induction and magnetic assembly parts, which matters for sensor, relay and magnetic clamping applications.
- Dimensional Stability After Forming: Low residual stress from controlled drawing keeps formed parts inside print tolerance after springback and stress relief.
- Traceable Batch Records: Every lot carries heat number, drawing date, tensile record and surface inspection result, issued as an EN 10204 3.1 certificate on request.
- Controlled {temper} Temper: The wire is drawn to Half Hard temper with a typical tensile range of 900-1,150 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
- {surf} Surface: A Bright Annealed finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
| Parameter | Specification |
|---|---|
| Steel Grade | 430 |
| Wire Diameter | 0.3 mm |
| Diameter Tolerance | ±0.01 mm |
| Surface Finish | Bright Annealed |
| Temper | Half Hard |
| Tensile Strength | 900-1,150 MPa |
| Chemical Composition | 16.0-18.0% Cr, max 0.12% C |
| Standard | EN 10088-3 |
| Coil Weight | 10 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | hearing aid components |
| Delivery Time | 15-25 days after deposit |
This Fine Stainless Steel Wire is specified where a supplier must guarantee the same mechanical result batch after batch, not just from a single sample. Buyers in hearing aid components use it because drawing schedule, surface condition and temper are held inside a narrow window, keeping forming tools and assembly fixtures stable across long production runs. Export programmes for hearing aid components demand consistent documentation and stable lead time. Production of this Fine Stainless Steel Wire is scheduled against a fixed rolling plan, with EN 10088-3 testing and dimensional reports issued before the container is sealed.
- Miniature relay springs
- Optical instrument springs
- Surgical suture needle wire
- Electronic connector contacts
- Medical guide wire and stylet
Packing follows 10 kg coil as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving. Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally 10 kg coil, and neutral packing with your own label is available for distributors.
Product Q&AQ: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.
Q: Which standard does this wire meet?
A: It is produced and tested against EN 10088-3, covering chemistry, dimensional tolerance, tensile properties and surface quality. Equivalent certificates to other national standards can be issued when your drawing references a different specification.
Q: What tensile range does Half Hard temper give?
A: For 430 at 0.3 in Half Hard temper the typical tensile range is 900-1,150 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.