6.0mm 430 Stainless Steel Straight Wire Half Hard Long Cycle Endurance
6.0mm 430 Straight Cut SS Wire
,Electrolysis Bright Straight Cut Wire
,Half Hard Wire Coil
The Electrolysis Bright finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming. Produced to JIS G4309, the wire pairs a Electrolysis Bright surface with a tensile range of 900-1,150 MPa, and every coil is traceable to its heat number. Each lot is supplied with a mill test certificate covering chemistry, tensile strength and dimensional inspection results.
Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record. Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders.
Key Features- Consistent Diameter Tolerance: Diameter is held to +/-0.03 mm across the whole coil and checked by laser micrometer every 50 m, so coiling and heading tools stay in setup without adjustment runs.
- Clean Degreased Coils: Coils are ultrasonically degreased and dried before packing, so plating or passivation lines need no extra pre cleaning step.
- Stable Magnetic Response: The 430 grade is ferromagnetic, which suits induction and magnetic assembly parts, which matters for sensor, relay and magnetic clamping applications.
- {surf} Surface: A Electrolysis Bright finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
- Controlled {temper} Temper: The wire is drawn to Half Hard temper with a typical tensile range of 900-1,150 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
- Verified Metallurgy: 430 chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
| Parameter | Specification |
|---|---|
| Steel Grade | 430 |
| Wire Diameter | 6.0 mm |
| Diameter Tolerance | ±0.03 mm |
| Surface Finish | Electrolysis Bright |
| Temper | Half Hard |
| Tensile Strength | 900-1,150 MPa |
| Chemical Composition | 16.0-18.0% Cr, max 0.12% C |
| Standard | JIS G4309 |
| Coil Weight | 20 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | dowel and shaft blanks |
| Delivery Time | 15-25 days after deposit |
Because dowel and shaft blanks often runs on high speed automatic equipment, wire that coils unevenly stops the line. The level winding and controlled cast of this Stainless Steel Straight Wire keep pay off tension constant, which is the practical reason repeat orders follow the first trial. Designers working on dowel and shaft blanks value the strength and ductility balance of 430 in Half Hard temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design.
- Decorative straight bars
- Grid and mesh welding
- Welding and filler applications
- Dowel and shaft blanks
- Electrode and terminal pins
Standard export packing is 20 kg coil per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low. Coils ship on 20 kg coil with a printed label showing heat number, diameter, temper and net weight, which makes goods receipt and FIFO rotation straightforward for buyers holding several grades in one store.
Product Q&AQ: Can you supply cut lengths instead of coils?
A: Yes. The wire can be straightened and cut to fixed lengths with square or deburred ends, packed in bundles or boxes. Cut length tolerance is normally plus or minus 1 mm, and closer control is available on request.
Q: Can the grade be substituted to reduce cost?
A: In dry indoor work 201 often replaces 304 at lower cost, and 430 suits magnetic or high temperature domestic parts. For chloride, marine or food contact service we keep 316 or 316L to protect the end user.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.