1.4mm 201 Stainless Steel Spring Wire Soap Coated Uniform Grain Structure
1.4mm 201 Spring Wire Coil
,Soap Coated SS Spring Wire
,Half Hard Wire Coil
The Soap Coated finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming. Typical service covers springs, wire forms and fasteners where both strength and corrosion resistance are required. Surface condition is monitored online, and finished coils are degreased before packing so plating lines receive clean material.
The wire is compatible with resistance welding, brazing and laser cutting, with no cracking at the fusion zone. Full traceability from melt to coil is maintained, including heat number, drawing date and final inspection signature.
Key Features- Straightness and Coil Build: Level wound or spooled packing keeps the wire tangle free, so automatic feeders run without stoppage caused by coil collapse.
- Custom Cut and Spool Options: Wire can be supplied on 15 kg coil, or cut to fixed lengths, matching your feeding equipment and stock policy.
- Consistent Diameter Tolerance: Diameter is held to +/-0.02 mm across the whole coil and checked by laser micrometer every 50 m, so coiling and heading tools stay in setup without adjustment runs.
- High Cycle Bending Endurance: Refined surface and clean microstructure reduce crack initiation sites, with sample lots tested beyond one million bending cycles.
- Fatigue Oriented Drawing: Multi pass drawing with intermediate annealing refines grain structure and limits inclusion stringers, extending fatigue life in cyclic spring and bending duty.
- Traceable Batch Records: Every lot carries heat number, drawing date, tensile record and surface inspection result, issued as an EN 10204 3.1 certificate on request.
| Parameter | Specification |
|---|---|
| Steel Grade | 201 |
| Wire Diameter | 1.4 mm |
| Diameter Tolerance | ±0.02 mm |
| Surface Finish | Soap Coated |
| Temper | Half Hard |
| Tensile Strength | 1,400-1,700 MPa |
| Chemical Composition | 16.0-18.0% Cr, 3.5-5.5% Ni, 5.5-7.5% Mn |
| Standard | GB/T 24588 |
| Coil Weight | 15 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | washing machine idler springs |
| Delivery Time | 15-25 days after deposit |
In washing machine idler springs the usual failure mode is fatigue or stress relaxation rather than simple overload. That is why this Stainless Steel Spring Wire is drawn from 201 with a refined grain structure and finished Soap Coated, so cyclic loading and warm service conditions do not shorten part life. Because washing machine idler springs often runs on high speed automatic equipment, wire that coils unevenly stops the line. The level winding and controlled cast of this Stainless Steel Spring Wire keep pay off tension constant, which is the practical reason repeat orders follow the first trial.
- Washing machine idler springs
- Watch band and jewellery springs
- Automotive return springs
- Medical and surgical instrument springs
- Small appliance latch springs
Coils ship on 15 kg coil with a printed label showing heat number, diameter, temper and net weight, which makes goods receipt and FIFO rotation straightforward for buyers holding several grades in one store. Packing follows 15 kg coil as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving.
Product Q&AQ: How is corrosion resistance verified?
A: Finished samples are tested by neutral salt spray to ASTM B117, and 201 chemistry is confirmed by spectrometry on each heat. For marine or chloride duty we recommend 316 or 316L rather than 304 or 201.
Q: Can the grade be substituted to reduce cost?
A: In dry indoor work 201 often replaces 304 at lower cost, and 430 suits magnetic or high temperature domestic parts. For chloride, marine or food contact service we keep 316 or 316L to protect the end user.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.