0.4mm 316 EPQ Stainless Steel Wire Bright Drawn Soft Annealed 15Kg Coil
0.4mm 316 EPQ Wire
,Bright Drawn EPQ Wire
,Soft Annealed Wire Coil
Typical service covers springs, wire forms and fasteners where both strength and corrosion resistance are required. Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section. Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders.
This EPQ Stainless Steel Wire is drawn from 316 stainless steel at 0.4 and supplied in Soft Annealed temper for buyers who need predictable forming behaviour. Produced to EN 10270-3, the wire pairs a Bright Drawn surface with a tensile range of 580-780 MPa, and every coil is traceable to its heat number.
Key Features- Stable Magnetic Response: The 316 grade is non-magnetic in the annealed condition, which matters for sensor, relay and magnetic clamping applications.
- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 316 grade is routinely supplied for food contact and drinking water adjacent parts.
- Fatigue Oriented Drawing: Multi pass drawing with intermediate annealing refines grain structure and limits inclusion stringers, extending fatigue life in cyclic spring and bending duty.
- Corrosion Performance: The 316 grade offers chloride and marine grade corrosion resistance from the molybdenum addition, verified by neutral salt spray testing of finished samples before dispatch.
- Traceable Batch Records: Every lot carries heat number, drawing date, tensile record and surface inspection result, issued as an EN 10204 3.1 certificate on request.
- Controlled {temper} Temper: The wire is drawn to Soft Annealed temper with a typical tensile range of 580-780 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
| Parameter | Specification |
|---|---|
| Steel Grade | 316 |
| Wire Diameter | 0.4 mm |
| Diameter Tolerance | ±0.01 mm |
| Surface Finish | Bright Drawn |
| Temper | Soft Annealed |
| Tensile Strength | 580-780 MPa |
| Chemical Composition | 16.0-18.0% Cr, 10.0-14.0% Ni, 2.0-3.0% Mo |
| Standard | EN 10270-3 |
| Coil Weight | 15 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | shower and tap fittings |
| Delivery Time | 15-25 days after deposit |
This EPQ Stainless Steel Wire is specified where a supplier must guarantee the same mechanical result batch after batch, not just from a single sample. Buyers in shower and tap fittings use it because drawing schedule, surface condition and temper are held inside a narrow window, keeping forming tools and assembly fixtures stable across long production runs. Purchasing teams sourcing for shower and tap fittings compare three things: dimensional consistency, surface cleanliness and documentation. This coil answers all three, with +/-0.01 mm diameter control, a degreased Bright Drawn surface and a heat number linked mill certificate for every lot.
- Shower and tap fittings
- Metal houseware frames
- Sanitary ware supports
- Kitchen rack and dish rack assemblies
- Elevator and handrail trim
Packing follows 15 kg coil as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving. Standard export packing is 15 kg coil per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low.
Product Q&AQ: Can the grade be substituted to reduce cost?
A: In dry indoor work 201 often replaces 304 at lower cost, and 430 suits magnetic or high temperature domestic parts. For chloride, marine or food contact service we keep 316 or 316L to protect the end user.
Q: What diameter tolerance can you hold on this EPQ Stainless Steel Wire?
A: Standard production holds +/-0.01 mm on the drawn diameter, checked with a laser micrometer at the start, middle and end of every coil. Tighter bands can be agreed for automatic coiling lines where feed finger clearance is critical.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.