0.8mm 201 EPQ Stainless Steel Wire Bright Drawn Half Hard Level Wound Coil
0.8mm 201 EPQ Wire Coil
,Bright Drawn EPQ Wire
,Half Hard Wire Coil
The Bright Drawn finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming. Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders. Produced to JIS G4309, the wire pairs a Bright Drawn surface with a tensile range of 1,400-1,700 MPa, and every coil is traceable to its heat number.
Coils are level wound with controlled cast and helix, so pay off tension stays even on automatic feeders. Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record.
Key Features- Verified Metallurgy: 201 chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
- Traceable Batch Records: Every lot carries heat number, drawing date, tensile record and surface inspection result, issued as an EN 10204 3.1 certificate on request.
- Welding and Fabrication Friendly: Balanced chemistry keeps the wire stable during resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
- Corrosion Performance: The 201 grade offers economical corrosion resistance for dry indoor and decorative duty, verified by neutral salt spray testing of finished samples before dispatch.
- Straightness and Coil Build: Level wound or spooled packing keeps the wire tangle free, so automatic feeders run without stoppage caused by coil collapse.
- Controlled {temper} Temper: The wire is drawn to Half Hard temper with a typical tensile range of 1,400-1,700 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
| Parameter | Specification |
|---|---|
| Steel Grade | 201 |
| Wire Diameter | 0.8 mm |
| Diameter Tolerance | ±0.01 mm |
| Surface Finish | Bright Drawn |
| Temper | Half Hard |
| Tensile Strength | 1,400-1,700 MPa |
| Chemical Composition | 16.0-18.0% Cr, 3.5-5.5% Ni, 5.5-7.5% Mn |
| Standard | JIS G4309 |
| Coil Weight | 20 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | display stand fabrication |
| Delivery Time | 15-25 days after deposit |
Designers working on display stand fabrication value the strength and ductility balance of 201 in Half Hard temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design. This EPQ Stainless Steel Wire is specified where a supplier must guarantee the same mechanical result batch after batch, not just from a single sample. Buyers in display stand fabrication use it because drawing schedule, surface condition and temper are held inside a narrow window, keeping forming tools and assembly fixtures stable across long production runs.
- Metal houseware frames
- Display stand fabrication
- Bathroom accessory frames
- Elevator and handrail trim
- Furniture wire frames
Packing follows 20 kg coil as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving. Standard export packing is 20 kg coil per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low.
Product Q&AQ: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.
Q: How is corrosion resistance verified?
A: Finished samples are tested by neutral salt spray to ASTM B117, and 201 chemistry is confirmed by spectrometry on each heat. For marine or chloride duty we recommend 316 or 316L rather than 304 or 201.
Q: Which standard does this wire meet?
A: It is produced and tested against JIS G4309, covering chemistry, dimensional tolerance, tensile properties and surface quality. Equivalent certificates to other national standards can be issued when your drawing references a different specification.