0.15mm 316L Stainless Steel Spring Wire Bright Drawn Spring Temper 1Kg Spool
0.15mm 316L Stainless Spring Wire
,Bright Drawn SS Spring Wire
,Spring Temper Wire Coil
Typical service covers springs, wire forms and fasteners where both strength and corrosion resistance are required. The 316L grade offers low carbon chloride resistance with reduced sensitisation at weld zones, which is the reason it is chosen for parts exposed to moisture, cleaning agents or repeated wash down. Surface condition is monitored online, and finished coils are degreased before packing so plating lines receive clean material.
Diameter control of +/-0.01 mm lets high speed coiling and heading equipment run without repeated tool adjustment between coils. Each lot is supplied with a mill test certificate covering chemistry, tensile strength and dimensional inspection results.
Key Features- Corrosion Performance: The 316L grade offers low carbon chloride resistance with reduced sensitisation at weld zones, verified by neutral salt spray testing of finished samples before dispatch.
- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 316L grade is routinely supplied for food contact and drinking water adjacent parts.
- Dimensional Stability After Forming: Low residual stress from controlled drawing keeps formed parts inside print tolerance after springback and stress relief.
- Custom Cut and Spool Options: Wire can be supplied on 1 kg spool, or cut to fixed lengths, matching your feeding equipment and stock policy.
- Controlled {temper} Temper: The wire is drawn to Spring Temper temper with a typical tensile range of 1,650-1,950 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
- Verified Metallurgy: 316L chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
| Parameter | Specification |
|---|---|
| Steel Grade | 316L |
| Wire Diameter | 0.15 mm |
| Diameter Tolerance | ±0.01 mm |
| Surface Finish | Bright Drawn |
| Temper | Spring Temper |
| Tensile Strength | 1,650-1,950 MPa |
| Chemical Composition | 16.0-18.0% Cr, 10.0-14.0% Ni, 2.0-3.0% Mo, max 0.03% C |
| Standard | ASTM A313/A313M |
| Coil Weight | 1 kg spool |
| Packing | VCI paper, strapping, wooden crate |
| Application | washing machine idler springs |
| Delivery Time | 15-25 days after deposit |
Purchasing teams sourcing for washing machine idler springs compare three things: dimensional consistency, surface cleanliness and documentation. This coil answers all three, with +/-0.01 mm diameter control, a degreased Bright Drawn surface and a heat number linked mill certificate for every lot. Designers working on washing machine idler springs value the strength and ductility balance of 316L in Spring Temper temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design.
- Small appliance latch springs
- Medical and surgical instrument springs
- Automotive return springs
- Watch band and jewellery springs
- Washing machine idler springs
Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally 1 kg spool, and neutral packing with your own label is available for distributors. Packing follows 1 kg spool as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving.
Product Q&AQ: Is customised chemistry or coating available?
A: Yes. We can adjust carbon and nitrogen within grade limits, apply soap, wax or polymer lubricant coatings, and print your brand on the spool flange for distributor programmes.
Q: What tensile range does Spring Temper temper give?
A: For 316L at 0.15 in Spring Temper temper the typical tensile range is 1,650-1,950 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.