logo

302 Spring Wire - Hydrogen Embrittlement After Plating

302 Spring Wire - Hydrogen Embrittlement After Plating
Properti Dasar
Tempat Asal: Tiongkok
Nama Merek: TOPONE
Sertifikasi: ISO/SGS/RosH
Nomor Model: 302
Properti Perdagangan
Jumlah Pesanan Minimum: 1000kg
Harga: Bisa dinegosiasikan
Ketentuan Pembayaran: T/T,L/C
Kemampuan Pasokan: > 1000 ton per bulan
Ringkasan Produk
302 Spring Wire - Hydrogen Embrittlement After Plating Stainless spring wire is chosen partly because it does not need a coating to resist corrosion. When a part is nevertheless plated, for appearance, solderability or a specific wear requirement, a new failure mode appears: hydrogen embrittlement. ...
Atribut Kustom Produk
Menyoroti

302 stainless steel spring wire

,

hydrogen embrittlement after plating

,

plated spring wire failure analysis

Sertifikasi:
ISO,SGS,Rosh
Aplikasi:
SPRING/SCREW/WIRE Form/Fishing
Diameter:
0,15-12mm
Bahan:
302
Permukaan:
Dilapisi Bright/Soap
Nama Produk:
1.5mm 302 Kawat Pegas Stainless Steel Cerah
Jenis:
Keras/lembut
Sedang mengemas:
gulungan, kumparan
Deskripsi Produk
Spesifikasi & Fitur Detail
302 Spring Wire - Hydrogen Embrittlement After Plating Stainless spring wire is chosen partly because it does not need a coating to resist corrosion. When a part is nevertheless plated, for appearance, solderability or a specific wear requirement, a new failure mode appears: hydrogen embrittlement. The hydrogen enters during pickling and during the plating itself, migrates to the regions of highest stress, and can cause a spring to break days after it was installed and passed