2.0mm 304 EPQ Stainless Steel Wire Soap Coated High Fatigue Life ASTM A580
304 stainless steel wire 2.0mm
,soap coated EPQ wire
,ASTM A580 high fatigue wire
Produced to ASTM A580, the wire pairs a Soap Coated surface with a tensile range of 600-800 MPa, and every coil is traceable to its heat number. The Soap Coated finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming. The wire is compatible with resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
This EPQ Stainless Steel Wire is drawn from 304 stainless steel at 2.0 and supplied in Soft Annealed temper for buyers who need predictable forming behaviour. Each lot is supplied with a mill test certificate covering chemistry, tensile strength and dimensional inspection results.
Key Features- Controlled {temper} Temper: The wire is drawn to Soft Annealed temper with a typical tensile range of 600-800 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
- Straightness and Coil Build: Level wound or spooled packing keeps the wire tangle free, so automatic feeders run without stoppage caused by coil collapse.
- {surf} Surface: A Soap Coated finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 304 grade is routinely supplied for food contact and drinking water adjacent parts.
- Dimensional Stability After Forming: Low residual stress from controlled drawing keeps formed parts inside print tolerance after springback and stress relief.
- Corrosion Performance: The 304 grade offers broad atmospheric and food contact corrosion resistance, verified by neutral salt spray testing of finished samples before dispatch.
| Parameter | Specification |
|---|---|
| Steel Grade | 304 |
| Wire Diameter | 2.0 mm |
| Diameter Tolerance | ±0.02 mm |
| Surface Finish | Soap Coated |
| Temper | Soft Annealed |
| Tensile Strength | 600-800 MPa |
| Chemical Composition | 18.0-20.0% Cr, 8.0-10.5% Ni |
| Standard | ASTM A580 |
| Coil Weight | 1 kg spool |
| Packing | VCI paper, strapping, wooden crate |
| Application | metal houseware frames |
| Delivery Time | 15-25 days after deposit |
In metal houseware frames the usual failure mode is fatigue or stress relaxation rather than simple overload. That is why this EPQ Stainless Steel Wire is drawn from 304 with a refined grain structure and finished Soap Coated, so cyclic loading and warm service conditions do not shorten part life. Designers working on metal houseware frames value the strength and ductility balance of 304 in Soft Annealed temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design.
- Display stand fabrication
- Furniture wire frames
- Sanitary ware supports
- Metal houseware frames
- Elevator and handrail trim
Packing follows 1 kg spool as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving. Coils ship on 1 kg spool with a printed label showing heat number, diameter, temper and net weight, which makes goods receipt and FIFO rotation straightforward for buyers holding several grades in one store.
Product Q&AQ: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.
Q: What diameter tolerance can you hold on this EPQ Stainless Steel Wire?
A: Standard production holds +/-0.02 mm on the drawn diameter, checked with a laser micrometer at the start, middle and end of every coil. Tighter bands can be agreed for automatic coiling lines where feed finger clearance is critical.
Q: Which standard does this wire meet?
A: It is produced and tested against ASTM A580, covering chemistry, dimensional tolerance, tensile properties and surface quality. Equivalent certificates to other national standards can be issued when your drawing references a different specification.