1.5mm 316L Stainless Steel Annealed Wire Consistent Springback 5Kg Coil
1.5mm 316L stainless steel wire
,annealed stainless steel wire coil
,5Kg stainless steel springback wire
The wire is compatible with resistance welding, brazing and laser cutting, with no cracking at the fusion zone. Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record. This Stainless Steel Annealed Wire is drawn from 316L stainless steel at 1.5 and supplied in Full Hard temper for buyers who need predictable forming behaviour.
Coils are level wound with controlled cast and helix, so pay off tension stays even on automatic feeders. Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section.
Key Features- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 316L grade is routinely supplied for food contact and drinking water adjacent parts.
- Verified Metallurgy: 316L chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
- Consistent Diameter Tolerance: Diameter is held to +/-0.02 mm across the whole coil and checked by laser micrometer every 50 m, so coiling and heading tools stay in setup without adjustment runs.
- Smooth Surface for Plating: Surface roughness is held below 0.8 micrometre on bright finishes, so nickel, chrome or PVD layers build evenly.
- {surf} Surface: A Matt Finish finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
- Welding and Fabrication Friendly: Balanced chemistry keeps the wire stable during resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
| Parameter | Specification |
|---|---|
| Steel Grade | 316L |
| Wire Diameter | 1.5 mm |
| Diameter Tolerance | ±0.02 mm |
| Surface Finish | Matt Finish |
| Temper | Full Hard |
| Tensile Strength | 1,850-2,150 MPa |
| Chemical Composition | 16.0-18.0% Cr, 10.0-14.0% Ni, 2.0-3.0% Mo, max 0.03% C |
| Standard | JIS G4309 |
| Coil Weight | 5 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | rivet and eyelet production |
| Delivery Time | 15-25 days after deposit |
This Stainless Steel Annealed Wire is specified where a supplier must guarantee the same mechanical result batch after batch, not just from a single sample. Buyers in rivet and eyelet production use it because drawing schedule, surface condition and temper are held inside a narrow window, keeping forming tools and assembly fixtures stable across long production runs. Export programmes for rivet and eyelet production demand consistent documentation and stable lead time. Production of this Stainless Steel Annealed Wire is scheduled against a fixed rolling plan, with JIS G4309 testing and dimensional reports issued before the container is sealed.
- Basket and rack fabrication
- Electrical resistance elements
- Kitchen utensil frames
- Rivet and eyelet production
- Ornamental wire craft
Coils ship on 5 kg coil with a printed label showing heat number, diameter, temper and net weight, which makes goods receipt and FIFO rotation straightforward for buyers holding several grades in one store. Packing follows 5 kg coil as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving.
Product Q&AQ: Do you provide first article inspection reports?
A: Yes. On request we issue a first article report covering diameter, ovality, tensile strength, surface condition and coil weight, together with the mill test certificate and heat number traceability.
Q: What diameter tolerance can you hold on this Stainless Steel Annealed Wire?
A: Standard production holds +/-0.02 mm on the drawn diameter, checked with a laser micrometer at the start, middle and end of every coil. Tighter bands can be agreed for automatic coiling lines where feed finger clearance is critical.
Q: What tensile range does Full Hard temper give?
A: For 316L at 1.5 in Full Hard temper the typical tensile range is 1,850-2,150 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.