0.5mm 201 Stainless Steel Annealed Wire Long Cycle Endurance 2Kg Spool
0.5mm 201 stainless steel wire
,annealed wire 2Kg spool
,long cycle endurance wire
The wire is compatible with resistance welding, brazing and laser cutting, with no cracking at the fusion zone. This Stainless Steel Annealed Wire is drawn from 201 stainless steel at 0.5 and supplied in Half Hard temper for buyers who need predictable forming behaviour. Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record.
Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section. Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders.
Key Features- Smooth Surface for Plating: Surface roughness is held below 0.8 micrometre on bright finishes, so nickel, chrome or PVD layers build evenly.
- Clean Degreased Coils: Coils are ultrasonically degreased and dried before packing, so plating or passivation lines need no extra pre cleaning step.
- Straightness and Coil Build: Level wound or spooled packing keeps the wire tangle free, so automatic feeders run without stoppage caused by coil collapse.
- Consistent Diameter Tolerance: Diameter is held to +/-0.01 mm across the whole coil and checked by laser micrometer every 50 m, so coiling and heading tools stay in setup without adjustment runs.
- High Cycle Bending Endurance: Refined surface and clean microstructure reduce crack initiation sites, with sample lots tested beyond one million bending cycles.
- Dimensional Stability After Forming: Low residual stress from controlled drawing keeps formed parts inside print tolerance after springback and stress relief.
| Parameter | Specification |
|---|---|
| Steel Grade | 201 |
| Wire Diameter | 0.5 mm |
| Diameter Tolerance | ±0.01 mm |
| Surface Finish | Electrolysis Bright |
| Temper | Half Hard |
| Tensile Strength | 1,400-1,700 MPa |
| Chemical Composition | 16.0-18.0% Cr, 3.5-5.5% Ni, 5.5-7.5% Mn |
| Standard | JIS G4309 |
| Coil Weight | 2 kg spool |
| Packing | VCI paper, strapping, wooden crate |
| Application | rivet and eyelet production |
| Delivery Time | 15-25 days after deposit |
Because rivet and eyelet production often runs on high speed automatic equipment, wire that coils unevenly stops the line. The level winding and controlled cast of this Stainless Steel Annealed Wire keep pay off tension constant, which is the practical reason repeat orders follow the first trial. This Stainless Steel Annealed Wire is specified where a supplier must guarantee the same mechanical result batch after batch, not just from a single sample. Buyers in rivet and eyelet production use it because drawing schedule, surface condition and temper are held inside a narrow window, keeping forming tools and assembly fixtures stable across long production runs.
- Wire bending and forming parts
- Electrical resistance elements
- Filter mesh reinforcement
- Basket and rack fabrication
- Hose clamp bands
Coils ship on 2 kg spool with a printed label showing heat number, diameter, temper and net weight, which makes goods receipt and FIFO rotation straightforward for buyers holding several grades in one store. Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally 2 kg spool, and neutral packing with your own label is available for distributors.
Product Q&AQ: What diameter tolerance can you hold on this Stainless Steel Annealed Wire?
A: Standard production holds +/-0.01 mm on the drawn diameter, checked with a laser micrometer at the start, middle and end of every coil. Tighter bands can be agreed for automatic coiling lines where feed finger clearance is critical.
Q: Can the grade be substituted to reduce cost?
A: In dry indoor work 201 often replaces 304 at lower cost, and 430 suits magnetic or high temperature domestic parts. For chloride, marine or food contact service we keep 316 or 316L to protect the end user.
Q: What tensile range does Half Hard temper give?
A: For 201 at 0.5 in Half Hard temper the typical tensile range is 1,400-1,700 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.