0.6mm 304 Stainless Steel Spring Wire High Fatigue Life ASTM A313/A313M
0.6mm 304 stainless spring wire
,ASTM A313/A313M spring wire
,high fatigue life spring wire
Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section. Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record. The Electrolysis Bright finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming.
Each lot is supplied with a mill test certificate covering chemistry, tensile strength and dimensional inspection results. Coils are level wound with controlled cast and helix, so pay off tension stays even on automatic feeders.
Key Features- Fatigue Oriented Drawing: Multi pass drawing with intermediate annealing refines grain structure and limits inclusion stringers, extending fatigue life in cyclic spring and bending duty.
- Custom Cut and Spool Options: Wire can be supplied on 100 kg drum, or cut to fixed lengths, matching your feeding equipment and stock policy.
- Controlled {temper} Temper: The wire is drawn to Half Hard temper with a typical tensile range of 1,300-1,600 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
- Smooth Surface for Plating: Surface roughness is held below 0.8 micrometre on bright finishes, so nickel, chrome or PVD layers build evenly.
- {surf} Surface: A Electrolysis Bright finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
- Welding and Fabrication Friendly: Balanced chemistry keeps the wire stable during resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
| Parameter | Specification |
|---|---|
| Steel Grade | 304 |
| Wire Diameter | 0.6 mm |
| Diameter Tolerance | ±0.01 mm |
| Surface Finish | Electrolysis Bright |
| Temper | Half Hard |
| Tensile Strength | 1,300-1,600 MPa |
| Chemical Composition | 18.0-20.0% Cr, 8.0-10.5% Ni |
| Standard | ASTM A313/A313M |
| Coil Weight | 100 kg drum |
| Packing | VCI paper, strapping, wooden crate |
| Application | battery contact springs |
| Delivery Time | 15-25 days after deposit |
In battery contact springs the usual failure mode is fatigue or stress relaxation rather than simple overload. That is why this Stainless Steel Spring Wire is drawn from 304 with a refined grain structure and finished Electrolysis Bright, so cyclic loading and warm service conditions do not shorten part life. Because battery contact springs often runs on high speed automatic equipment, wire that coils unevenly stops the line. The level winding and controlled cast of this Stainless Steel Spring Wire keep pay off tension constant, which is the practical reason repeat orders follow the first trial.
- Battery contact springs
- Medical and surgical instrument springs
- Telecom connector springs
- Small appliance latch springs
- Sprayer and lotion pump springs
Coils ship on 100 kg drum with a printed label showing heat number, diameter, temper and net weight, which makes goods receipt and FIFO rotation straightforward for buyers holding several grades in one store. Packing follows 100 kg drum as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving.
Product Q&AQ: Is the surface suitable for electroplating or PVD?
A: Yes. Bright finishes are degreased with surface roughness below 0.8 micrometre, so nickel, chrome or PVD layers build evenly. Soap coated wire needs a light alkaline clean before plating.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.
Q: How is corrosion resistance verified?
A: Finished samples are tested by neutral salt spray to ASTM B117, and 304 chemistry is confirmed by spectrometry on each heat. For marine or chloride duty we recommend 316 or 316L rather than 304 or 201.