3.0mm 316L Stainless Steel Straight Wire Bright Drawn Half Hard JIS G4309
3.0mm 316L Straight Cut Wire
,Bright Drawn Straight Cut Wire
,Half Hard Wire Coil
Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record. Drawing is carried out on multi pass lines with intermediate annealing, so grain structure stays fine and uniform through the section. The 316L grade offers low carbon chloride resistance with reduced sensitisation at weld zones, which is the reason it is chosen for parts exposed to moisture, cleaning agents or repeated wash down.
The Bright Drawn finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming. Full traceability from melt to coil is maintained, including heat number, drawing date and final inspection signature.
Key Features- Custom Cut and Spool Options: Wire can be supplied on 5 kg coil, or cut to fixed lengths, matching your feeding equipment and stock policy.
- Verified Metallurgy: 316L chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
- {surf} Surface: A Bright Drawn finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
- Traceable Batch Records: Every lot carries heat number, drawing date, tensile record and surface inspection result, issued as an EN 10204 3.1 certificate on request.
- Dimensional Stability After Forming: Low residual stress from controlled drawing keeps formed parts inside print tolerance after springback and stress relief.
- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 316L grade is routinely supplied for food contact and drinking water adjacent parts.
| Parameter | Specification |
|---|---|
| Steel Grade | 316L |
| Wire Diameter | 3.0 mm |
| Diameter Tolerance | ±0.02 mm |
| Surface Finish | Bright Drawn |
| Temper | Half Hard |
| Tensile Strength | 1,200-1,500 MPa |
| Chemical Composition | 16.0-18.0% Cr, 10.0-14.0% Ni, 2.0-3.0% Mo, max 0.03% C |
| Standard | JIS G4309 |
| Coil Weight | 5 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | decorative straight bars |
| Delivery Time | 15-25 days after deposit |
Because decorative straight bars often runs on high speed automatic equipment, wire that coils unevenly stops the line. The level winding and controlled cast of this Stainless Steel Straight Wire keep pay off tension constant, which is the practical reason repeat orders follow the first trial. Designers working on decorative straight bars value the strength and ductility balance of 316L in Half Hard temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design.
- Grid and mesh welding
- Welding and filler applications
- Needle and probe blanks
- Decorative straight bars
- Cnc cut to length pin production
Packing follows 5 kg coil as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving. Standard export packing is 5 kg coil per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low.
Product Q&AQ: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.
Q: How do you prevent coil collapse during unwinding?
A: Coils are level wound with controlled cast and helix, then restrained with strapping and VCI film. For high speed feeders we recommend spooled packing, which keeps pay off tension constant.
Q: Is the surface suitable for electroplating or PVD?
A: Yes. Bright finishes are degreased with surface roughness below 0.8 micrometre, so nickel, chrome or PVD layers build evenly. Soap coated wire needs a light alkaline clean before plating.