3.0mm 316 Stainless Steel Straight Wire Soap Coated Soft Annealed JIS G4309
3.0mm 316 Straight Cut SS Wire
,Soap Coated Straight Cut Wire
,Soft Annealed Wire Coil
This Stainless Steel Straight Wire is drawn from 316 stainless steel at 3.0 and supplied in Soft Annealed temper for buyers who need predictable forming behaviour. Surface condition is monitored online, and finished coils are degreased before packing so plating lines receive clean material. The wire is compatible with resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record. Produced to JIS G4309, the wire pairs a Soap Coated surface with a tensile range of 580-780 MPa, and every coil is traceable to its heat number.
Key Features- Verified Metallurgy: 316 chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
- Smooth Surface for Plating: Surface roughness is held below 0.8 micrometre on bright finishes, so nickel, chrome or PVD layers build evenly.
- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 316 grade is routinely supplied for food contact and drinking water adjacent parts.
- Welding and Fabrication Friendly: Balanced chemistry keeps the wire stable during resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
- Corrosion Performance: The 316 grade offers chloride and marine grade corrosion resistance from the molybdenum addition, verified by neutral salt spray testing of finished samples before dispatch.
- Consistent Diameter Tolerance: Diameter is held to +/-0.02 mm across the whole coil and checked by laser micrometer every 50 m, so coiling and heading tools stay in setup without adjustment runs.
| Parameter | Specification |
|---|---|
| Steel Grade | 316 |
| Wire Diameter | 3.0 mm |
| Diameter Tolerance | ±0.02 mm |
| Surface Finish | Soap Coated |
| Temper | Soft Annealed |
| Tensile Strength | 580-780 MPa |
| Chemical Composition | 16.0-18.0% Cr, 10.0-14.0% Ni, 2.0-3.0% Mo |
| Standard | JIS G4309 |
| Coil Weight | 10 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | needle and probe blanks |
| Delivery Time | 15-25 days after deposit |
Purchasing teams sourcing for needle and probe blanks compare three things: dimensional consistency, surface cleanliness and documentation. This coil answers all three, with +/-0.02 mm diameter control, a degreased Soap Coated surface and a heat number linked mill certificate for every lot. Designers working on needle and probe blanks value the strength and ductility balance of 316 in Soft Annealed temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design.
- Electrode and terminal pins
- Decorative straight bars
- Grid and mesh welding
- Cnc cut to length pin production
- Welding and filler applications
Standard export packing is 10 kg coil per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low. Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally 10 kg coil, and neutral packing with your own label is available for distributors.
Product Q&AQ: Do you provide first article inspection reports?
A: Yes. On request we issue a first article report covering diameter, ovality, tensile strength, surface condition and coil weight, together with the mill test certificate and heat number traceability.
Q: What tensile range does Soft Annealed temper give?
A: For 316 at 3.0 in Soft Annealed temper the typical tensile range is 580-780 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.