7.0mm 304 EPQ Stainless Steel Wire Bright Annealed Spring Temper GB/T 24588
7.0mm 304 EPQ Wire
,Bright Annealed EPQ Wire
,Spring Temper Wire Coil
Typical service covers springs, wire forms and fasteners where both strength and corrosion resistance are required. Produced to GB/T 24588, the wire pairs a Bright Annealed surface with a tensile range of 1,700-2,000 MPa, and every coil is traceable to its heat number. This EPQ Stainless Steel Wire is drawn from 304 stainless steel at 7.0 and supplied in Spring Temper temper for buyers who need predictable forming behaviour.
Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders. Surface condition is monitored online, and finished coils are degreased before packing so plating lines receive clean material.
Key Features- Welding and Fabrication Friendly: Balanced chemistry keeps the wire stable during resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
- {surf} Surface: A Bright Annealed finish keeps the surface free of drawing lines, die marks and trapped lubricant, which protects plating adhesion and reduces tool wear.
- Smooth Surface for Plating: Surface roughness is held below 0.8 micrometre on bright finishes, so nickel, chrome or PVD layers build evenly.
- Stable Magnetic Response: The 304 grade is essentially non-magnetic in the annealed condition, which matters for sensor, relay and magnetic clamping applications.
- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 304 grade is routinely supplied for food contact and drinking water adjacent parts.
- Fatigue Oriented Drawing: Multi pass drawing with intermediate annealing refines grain structure and limits inclusion stringers, extending fatigue life in cyclic spring and bending duty.
| Parameter | Specification |
|---|---|
| Steel Grade | 304 |
| Wire Diameter | 7.0 mm |
| Diameter Tolerance | ±0.03 mm |
| Surface Finish | Bright Annealed |
| Temper | Spring Temper |
| Tensile Strength | 1,700-2,000 MPa |
| Chemical Composition | 18.0-20.0% Cr, 8.0-10.5% Ni |
| Standard | GB/T 24588 |
| Coil Weight | 5 kg coil |
| Packing | VCI paper, strapping, wooden crate |
| Application | elevator and handrail trim |
| Delivery Time | 15-25 days after deposit |
Designers working on elevator and handrail trim value the strength and ductility balance of 304 in Spring Temper temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design. In elevator and handrail trim the usual failure mode is fatigue or stress relaxation rather than simple overload. That is why this EPQ Stainless Steel Wire is drawn from 304 with a refined grain structure and finished Bright Annealed, so cyclic loading and warm service conditions do not shorten part life.
- Display stand fabrication
- Elevator and handrail trim
- Shower and tap fittings
- Metal houseware frames
- Sanitary ware supports
Each coil is wrapped in VCI paper, tied with plastic strapping and packed in a wooden crate or on a fumigated pallet. Coil weight is normally 5 kg coil, and neutral packing with your own label is available for distributors. Standard export packing is 5 kg coil per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low.
Product Q&AQ: Is the surface suitable for electroplating or PVD?
A: Yes. Bright finishes are degreased with surface roughness below 0.8 micrometre, so nickel, chrome or PVD layers build evenly. Soap coated wire needs a light alkaline clean before plating.
Q: Do you provide first article inspection reports?
A: Yes. On request we issue a first article report covering diameter, ovality, tensile strength, surface condition and coil weight, together with the mill test certificate and heat number traceability.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.