1.2mm 304 EPQ Stainless Steel Wire Bright Drawn Low Residual Stress GB/T 24588
1.2mm 304 Stainless EPQ Wire
,Bright Drawn EPQ Wire
,Spring Temper Wire Coil
Batches are held to the same drawing schedule, which is why customers see the same springback value across repeat orders. Diameter control of +/-0.02 mm lets high speed coiling and heading equipment run without repeated tool adjustment between coils. Chemistry is verified by optical emission spectrometry on each heat, and dimensional checks are logged with the coil record.
The Bright Drawn finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming. Full traceability from melt to coil is maintained, including heat number, drawing date and final inspection signature.
Key Features- Controlled {temper} Temper: The wire is drawn to Spring Temper temper with a typical tensile range of 1,700-2,000 MPa, giving repeatable springback and forming behaviour from the first metre to the last.
- Dimensional Stability After Forming: Low residual stress from controlled drawing keeps formed parts inside print tolerance after springback and stress relief.
- Corrosion Performance: The 304 grade offers broad atmospheric and food contact corrosion resistance, verified by neutral salt spray testing of finished samples before dispatch.
- Stable Magnetic Response: The 304 grade is essentially non-magnetic in the annealed condition, which matters for sensor, relay and magnetic clamping applications.
- Clean Degreased Coils: Coils are ultrasonically degreased and dried before packing, so plating or passivation lines need no extra pre cleaning step.
- Consistent Diameter Tolerance: Diameter is held to +/-0.02 mm across the whole coil and checked by laser micrometer every 50 m, so coiling and heading tools stay in setup without adjustment runs.
| Parameter | Specification |
|---|---|
| Steel Grade | 304 |
| Wire Diameter | 1.2 mm |
| Diameter Tolerance | ±0.02 mm |
| Surface Finish | Bright Drawn |
| Temper | Spring Temper |
| Tensile Strength | 1,700-2,000 MPa |
| Chemical Composition | 18.0-20.0% Cr, 8.0-10.5% Ni |
| Standard | GB/T 24588 |
| Coil Weight | Z2 coil on cardboard core |
| Packing | VCI paper, strapping, wooden crate |
| Application | sanitary ware supports |
| Delivery Time | 15-25 days after deposit |
Designers working on sanitary ware supports value the strength and ductility balance of 304 in Spring Temper temper. Parts can be formed close to the minimum bend radius without edge cracking, and springback stays predictable enough to be compensated in the tool design. In sanitary ware supports the usual failure mode is fatigue or stress relaxation rather than simple overload. That is why this EPQ Stainless Steel Wire is drawn from 304 with a refined grain structure and finished Bright Drawn, so cyclic loading and warm service conditions do not shorten part life.
- Shower and tap fittings
- Kitchen rack and dish rack assemblies
- Sanitary ware supports
- Display stand fabrication
- Elevator and handrail trim
Packing follows Z2 coil on cardboard core as the base unit, with moisture barrier film and desiccant inside the crate for sea freight. Container loading photos and a packing list are issued before shipment so your warehouse can plan receiving. Coils ship on Z2 coil on cardboard core with a printed label showing heat number, diameter, temper and net weight, which makes goods receipt and FIFO rotation straightforward for buyers holding several grades in one store.
Product Q&AQ: What tensile range does Spring Temper temper give?
A: For 304 at 1.2 in Spring Temper temper the typical tensile range is 1,700-2,000 MPa. A mill test certificate with the measured value for each heat is issued with the shipment.
Q: What is the minimum order quantity and lead time?
A: A trial order from 500 kg per size is accepted so you can validate forming behaviour. Repeat production quantities ship in 15 to 25 days after deposit, and stock sizes move within a week.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.