0.9mm 304 Stainless Steel Spring Wire Spring Temper Long Cycle Endurance
0.9mm 304 Spring Wire Coil
,Bright Annealed SS Spring Wire
,Spring Temper Wire Coil
Coils are level wound with controlled cast and helix, so pay off tension stays even on automatic feeders. Surface condition is monitored online, and finished coils are degreased before packing so plating lines receive clean material. Produced to ASTM A313/A313M, the wire pairs a Bright Annealed surface with a tensile range of 1,700-2,000 MPa, and every coil is traceable to its heat number.
The Bright Annealed finish is applied under controlled lubrication, which limits die marks and keeps friction stable during forming. Each lot is supplied with a mill test certificate covering chemistry, tensile strength and dimensional inspection results.
Key Features- Fatigue Oriented Drawing: Multi pass drawing with intermediate annealing refines grain structure and limits inclusion stringers, extending fatigue life in cyclic spring and bending duty.
- Consistent Diameter Tolerance: Diameter is held to +/-0.01 mm across the whole coil and checked by laser micrometer every 50 m, so coiling and heading tools stay in setup without adjustment runs.
- Welding and Fabrication Friendly: Balanced chemistry keeps the wire stable during resistance welding, brazing and laser cutting, with no cracking at the fusion zone.
- Verified Metallurgy: 304 chemistry is confirmed by optical emission spectrometry on every heat, and each coil carries a heat number linked to the mill test certificate.
- RoHS and Food Contact Ready: Material complies with RoHS and REACH, and the 304 grade is routinely supplied for food contact and drinking water adjacent parts.
- Straightness and Coil Build: Level wound or spooled packing keeps the wire tangle free, so automatic feeders run without stoppage caused by coil collapse.
| Parameter | Specification |
|---|---|
| Steel Grade | 304 |
| Wire Diameter | 0.9 mm |
| Diameter Tolerance | ±0.01 mm |
| Surface Finish | Bright Annealed |
| Temper | Spring Temper |
| Tensile Strength | 1,700-2,000 MPa |
| Chemical Composition | 18.0-20.0% Cr, 8.0-10.5% Ni |
| Standard | ASTM A313/A313M |
| Coil Weight | 100 kg drum |
| Packing | VCI paper, strapping, wooden crate |
| Application | medical and surgical instrument springs |
| Delivery Time | 15-25 days after deposit |
Purchasing teams sourcing for medical and surgical instrument springs compare three things: dimensional consistency, surface cleanliness and documentation. This coil answers all three, with +/-0.01 mm diameter control, a degreased Bright Annealed surface and a heat number linked mill certificate for every lot. This Stainless Steel Spring Wire is specified where a supplier must guarantee the same mechanical result batch after batch, not just from a single sample. Buyers in medical and surgical instrument springs use it because drawing schedule, surface condition and temper are held inside a narrow window, keeping forming tools and assembly fixtures stable across long production runs.
- Sprayer and lotion pump springs
- Washing machine idler springs
- Door lock springs
- Small appliance latch springs
- Battery contact springs
Standard export packing is 100 kg drum per coil, protected by VCI film and edge protectors, then palletised for forklift handling. A twenty foot container loads up to 22 tonnes when coils are nested, keeping freight cost per tonne low. Coils ship on 100 kg drum with a printed label showing heat number, diameter, temper and net weight, which makes goods receipt and FIFO rotation straightforward for buyers holding several grades in one store.
Product Q&AQ: Do you provide first article inspection reports?
A: Yes. On request we issue a first article report covering diameter, ovality, tensile strength, surface condition and coil weight, together with the mill test certificate and heat number traceability.
Q: Can you supply cut lengths instead of coils?
A: Yes. The wire can be straightened and cut to fixed lengths with square or deburred ends, packed in bundles or boxes. Cut length tolerance is normally plus or minus 1 mm, and closer control is available on request.
Q: Which temper should I choose for spring parts?
A: Spring temper for maximum elastic recovery, half hard where forming severity is high, and soft annealed where the part is bent or deep formed before hardening. Trial coils in two tempers are available so your tool room can compare.