logo

Fatigue Resistant 302 Spring Wire 2.5 mm Compression Spring Spool

Fatigue Resistant 302 Spring Wire 2.5 mm Compression Spring Spool
Basic Properties
Place of Origin: China
Brand Name: Toponewire
Certification: ISO9001:2015
Model Number: SUS 302
Trading Properties
Minimum Order Quantity: Negotiation
Price: Negotiable
Payment Terms: T/T, L/C, D/A, D/P
Supply Ability: 500 tons per month
Product Summary
Fatigue resistant 302 spring wire at 2.5 mm on spools, with surface and microstructure control for compression springs under repeated load.
Product Custom Attributes
Highlight

302 spring wire 2.5 mm

,

fatigue resistant compression spring

,

stainless steel spring wire spool

Material:
SUS 302 / AISI 302
Standard:
JIS G. EN10270-3. ASTM. DIN. GB Etc
Surface:
Soap Coated / Bright
Packing:
Coil Or Spool With Plate
Coil Inner Diameter:
250-1000mm
Supply Ability:
>500 Tons Per Month
Product Description
Detailed Specifications & Features

Most compression springs do not fail on the first load. They fail after a hundred thousand or a million cycles, starting from a small surface irregularity where stress concentrates. Building fatigue resistance into 302 spring wire therefore means controlling what happens at the surface and just below it, not only what the tensile test reports.

For the 2.5 mm fatigue resistant wire we pay attention to three things. First, cleanness: non metallic inclusions near the surface act as initiation sites, so the steel is selected and the drawing route arranged to keep the surface skin clean. Second, surface integrity: die condition is monitored so laps and scoring are avoided. Third, residual stress: the drawing and stress relief sequence is set to leave the wire in a condition that behaves predictably when the spring is coiled and compressed.

The result is a compression spring wire that performs consistently in applications with repeated cycling, such as valves, pumps, dampers and mechanical linkages, where a spring that loses force or breaks early stops the whole assembly.

Key Features
  • Clean Surface Skin: Inclusion control and die monitoring reduce the surface irregularities that start fatigue cracks in a compression spring.
  • Residual Stress Control: Drawing and stress relief are sequenced so the finished 302 stainless steel spring wire behaves predictably under cyclic compression.
  • Spool Packing: 2.5 mm wire on spools feeds smoothly into CNC coilers and keeps tension constant across a long production run.
  • Stable Tensile: A reported tensile band supports consistent spring rate, so force loss over life can be assessed with confidence.
  • Consistent Diameter: Diameter is held within the agreed tolerance, which keeps the spring index and the stress calculation valid.
  • Coating Options: Bright or soap coated surfaces are available, so friction at the coiler can be matched to the forming process.
Technical Specifications
ParameterSpecification
Material GradeAISI 302 austenitic stainless steel
Nominal Diameter2.5 mm, range 0.30 - 8 mm available
Delivery ConditionCold drawn spring temper
Tensile StrengthReported per lot, per diameter and temper
SurfaceBright drawn or soap coated
Inclusion ControlSurface skin inspected, suspect lengths removed
Coil FormSpool or plate packed coil
Spool Payload10 - 100 kg per spool, agreed per order
Applicable StandardsEN 10270-3, ASTM A313, JIS G4314
PackingSpool on pallet with moisture barrier
Applications

Repeated load applications define this group. Where a spring is compressed thousands of times per shift, fatigue life becomes the design driver and surface quality matters as much as the nominal strength of the wire.

  • Valve and pump springs under continuous cycling
  • Damper and suspension springs in machinery
  • Springs in reciprocating mechanical linkages
  • Springs in compressors and pneumatic tools
  • Return springs in automated production equipment
  • Springs in safety and locking mechanisms with frequent actuation
Packaging & Quality Assurance

The 2.5 mm fatigue resistant wire is supplied on spools or plate packed coils with a moisture barrier, labelled with grade, diameter, temper, tensile result and lot number. Our ISO9001:2015 system includes surface inspection, diameter measurement and mechanical testing, with results retained against the lot. For springs with a defined cycle target, we recommend a short fatigue or endurance run on sample coils, since the completed spring geometry and the shot peening or stress relief step have as much influence on life as the incoming wire.

Frequently Asked Questions What determines fatigue life in a compression spring?

Stress range, surface quality, residual stress and the number of cycles all contribute. Wire with a clean surface removes the most common crack initiation site, but spring geometry still has to be designed within sensible stress limits.

Is shot peening necessary for stainless springs?

It is a common way to introduce compressive residual stress at the surface and extend life in highly stressed springs. Whether it is needed depends on the stress range and the required cycle count.

Can you supply fatigue test data with the wire?

We report tensile, elongation and surface inspection results per lot. Component level fatigue testing is normally carried out on finished springs, and we can support a sample run.

Why is spool packing used at 2.5 mm?

A spool keeps tension constant and lets a long production run continue without stopping to change a coil, which also reduces the risk of handling damage to the wire surface.

What information helps you recommend a wire condition?

Tell us the spring dimensions, the stress range, the required cycle life and the forming process. That allows the temper and surface finish to be matched to the actual duty.